Halayen Aikin Samfurin
Mai sauƙin muhalli da ƙarancin carbon
Aikin injiniya yayi daidai da fina-finan BOPA na gargajiya
Mafi kyawun daidaito da lamination 


Shawarar Yanayin Sarrafawa | Samfuri (kauri) | Surface na Corona | Ƙarfin bugawa | Tsarin akwati | Faɗin hatimi | Juriyar Juyawar Juyawar |
| TSA-15μm | Mutum ɗaya/biyu | Launuka ≤3 | Ba a ba da shawarar ba | ≤1 | ≤100℃ (ƙaramin guda ɗaya) |
| ≤121℃ (ƙananan ƙwayoyin cuta biyu) | |||||
| TSar-15μm | Mutum ɗaya/biyu | ≤9 launuka | Akwai | ≤6 | ≤121℃ |
Babban Sigogi na Fasaha (15μm) | Abubuwan Gwaji | Matsakaicin Darajar | Ka'idojin Gwaji | Abubuwan Gwaji | Matsayin gwaji | Matsakaicin Darajar |
| (MD/TD) Ƙarfin tauri | 200/230MPa | GB/T 1040.3-2006 | Tashin hankali a saman (coron guda ɗaya) Tashin hankali a saman (coronal biyu) | GB/T 14216-2008 | An yi wa magani 54/ba a yi wa magani ba 39 mN/m ciki 54/waje 50 mN/m |
| (MD/TD) Ƙarfin tensile mara iyaka |
| GB/T 1040.3-2006 | |||
| Ƙarfin juriyar huda | 10 N | GB/T 10004-2008 | Ma'aunin daidaitawa (tsaye/tsauri, mara/babu) | GB/T 10006-2021 | 0.50/0.35 |
| (MD/TD)(160℃, minti 5) Ƙarfin raguwar zafi | ≤4.0%/≤3.0% | GB/T 12027-2004 | Lambar lasisin TSA Kabut TSAr | GB/T 2410-2008 | 3.5% 3.0% |
| Tashin hankali a saman (coron guda ɗaya) Tashin hankali a saman (coronal biyu) | An yi wa magani 54/ba a yi wa magani ba 39 mN/m ciki 54/waje 50 mN/m | GB/T 14216-2008 | (23℃, 50% RH) Yawan watsa iskar oxygen | GB/T 1038-2022 | 55 cc/(㎡.rana.atm) |
| Ma'aunin daidaitawa (tsaye/tsauri, mara/babu) | 0.60/0.45 | GB/T 10006-2021 | |||
| hazo | 4.5% | GB/T 2410-2008 |
Bayanan Daidaitacce | Samfuri (kauri) | Tsawon birgima/m | Faɗin Ragewa na Daidaitacce/mm | Ukuran paper core/in | Marufi |
| BioOPA-15μm | 6000 | 300-1200 | 3 | Raka'a 9/pallet |
| 12000 | 6 | Raka'a 4/pallet |